SFA/AWS A5.14 |
ERNiCrMo-3 |
EN ISO 18274 |
S Ni 6625 (NiCr22Mo9Nb) |
測試溫度(焊態(tài)) | +20 °C |
結(jié)果(焊態(tài)) | 130 J |
測試溫度(焊態(tài)) | -105 °C |
結(jié)果(焊態(tài)) | 120 J |
伸長率(焊態(tài)) | 40 % |
屈服強(qiáng)度(焊態(tài)) | 550 MPa |
抗拉強(qiáng)度(焊態(tài)) | 780 MPa |
電流類型 CA/CD/CC (+)(-) | DC(-) |
直徑 | 1.6 mm |
直徑 | 2 mm |
A nickel-based, corrosion- and heat-resistant, 22% Cr, 9% Mo, 3.5% Nb rod for the GTAW of high-alloyed steel, heat-resistant steel, corrosion-resistant steel, 9% Ni steels and similar steel with high notch toughness at low temperatures. It is also suitable for joining dissimilar bls of the types mentioned above. OK Tigrod 19.82 is normally welded with pure Ar as the shielding gas.