熔體流動(dòng)速率 | 3.5 | g/10min | ASTM D-1238 |
收縮率 | 1.5-2.0 | % | SK |
斷裂伸長率 | >500 | % | ASTM D-638 |
IZOD缺口沖擊強(qiáng)度 (23℃) | 16 | kg.cm/cm | ASTM D-256 |
表面硬度 | 80 | R scale | ASTM D-785 |
斷裂拉伸強(qiáng)度 | 280 | Kg/cm | ASTM D-638 |
IZOD缺口沖擊強(qiáng)度 (-20℃) | 5 | kg.cm/cm | ASTM D-256 |
彈性彎曲系數(shù) | 14000 | Kg/cm | ASTM D-790 |
熱變形溫度 | 98 | ℃ | ASTM D-648 |
維卡軟化點(diǎn) | 150 | ℃ | ASTM D-1525 |
加速老化時(shí)間 | 360 | hr | ASTM D-3012 |
流動(dòng)性 | 550 | mm | SK |