比重 | DAM|50%RH1.14|1.14 | ASTM D-792 |
洛氏硬度R | DAM|50%RHR123|- | ASTM D-785 | |
斷裂伸長率 (23℃) | DAM|50%RH25|100 | % | ASTM D-638 |
埃佐沖擊強度 (23℃) | DAM|50%RH37|64 | j/m | ASTM D-256 |
揉曲模量 (23℃) | DAM|50%RH3020|1779 | MPa | ASTM D-790 |
拉伸強度 (23℃) | DAM|50%RH97.9|70.3 | MPa | ASTM D-638 |
熔點 (Fisher Johns法) | DAM|50%RH256|256 | ℃ | ASTM D-789 |
熱畸變溫度 | ASTM D-648 | ||
((0.5)×10Pa) | DAM|50%RH242|- | ℃ | |
(18×10Pa) | DAM|50%RH90|- | ℃ | |
UL可燃性導(dǎo)級 | DAM|50%RH94|V-2 |