沖擊強(qiáng)度缺口 (23℃) | 533 | J/m | ASTM D-256 |
模具收縮率 (3.2mm) | 4-7 | E-3 | ASTM D-955 |
吸水率 | 0.1 | % | ASTM D-570 |
比重 | 1.13 | ASTM D-792 |
拉伸率(斷裂點(diǎn)) | 100 | % | ASTM D-638 |
拉伸模量 | 2067 | MPa | ASTM D-638 |
彎曲模量 | 2067 | MPa | ASTM D-790 |
拉伸強(qiáng)度(屈伏點(diǎn)) | 52 | MPa | ASTM D-638 |
熱變形溫度 (0.45Mpa) | 123 | ℃ | ASTM D-648 |
彎曲強(qiáng)度 | 77 | MPa | ASTM D-790 |
線膨脹系數(shù) | 8.1E-05 | 1/℃ | ASTM E-831 |
熱變形溫度 (1.8Mpa) | 104 | ℃ | ASTM D-648 |