比重 | 1.56 | ASTM D792 | |
吸水率 | 0.2 | % | ASTM D570 |
縮模率 | |||
(平行方向) | 0.4-05 | % | |
(垂直方向) | 1.0-1.2 | % |
拉伸強(qiáng)度 | 127 | MPa | ASTM D638 |
延伸率 | 3 | % | ASTM D638 |
彎曲強(qiáng)度 | 196 | MPa | ASTM D790 |
彎曲模量 | 8230 | MPa | ASTM D790 |
IZOD缺口沖擊強(qiáng)度 | 78 | J/M | ASTM D256 |
洛氏硬度 | ASTM D785 | ||
90 | M | ||
120 | R | ||
磨耗 | 23 | ASTM D1044 |
熔融指數(shù) | 10 | g/10min | ASTM D1238 |
線膨脹系數(shù) | 4/9 | ||
熱變形溫度 | ASTM D648 | ||
(1.82MPa) | 170 | ℃ | |
(0.45MPa) | 174 | ℃ | |
阻燃性 | HB |