吸濕率 | 0.2 | % | ASTM D-570 |
熔體流動(dòng)速率 | 30 | gr/10min | ASTM D-1238 |
成型收縮率 | 1.6-2.0 | % | 旭化成方法 |
磨耗率 | 14 | mg/1000次 | ASTM D-1044 |
比重 | 1.41 | ASTM D-792 |
延伸率 | 50 | % | ASTM D-638 |
洛氏硬度 | 80 | M scale | ASTM D-785 |
抗撓系數(shù) | 2630 | MPa | ASTM D-790 |
洛氏硬度 | 115 | R scale | ASTM D-785 |
抗撓強(qiáng)度 | 90 | MPa | ASTM D-790 |
拉伸強(qiáng)度 | 61 | MPa | ASTM D-638 |
懸臂梁式缺口沖擊強(qiáng)度 | 59 | J/M | ASTM D-256 |
熱變形溫度 | ASTM D-645 | ||
(0.45MPa) | 158 | ℃ | |
(1.82MPa) | 110 | ℃ | |
阻燃性 | HB | UL 94 | |
線性膨脹系數(shù) | 10 | ×10-5cm/cm℃ | TMA |