Grade : | 2326 鐵素體壓力不銹鋼棒 | |||||||
Number: | X2CrMoTi18-2 | |||||||
Classification: | 鐵素體不銹鋼 | |||||||
Density: | 7.7 g/cm 3 | |||||||
Standard: | ||||||||
EN 10088-2:2005不銹鋼。通用耐腐蝕鋼片/板和帶材交貨技術(shù)條件 | ||||||||
EN 10028-7:2007壓力用鋼制扁平產(chǎn)品。不銹鋼 | ||||||||
EN 10296-2:2005機(jī)械和一般工程用焊接圓鋼管。不銹鋼。技術(shù)交付條件 | ||||||||
EN 10088-1:2005不銹鋼。不銹鋼清單 | ||||||||
EN 10088-4:2009不銹鋼。建筑用耐腐蝕鋼片/板和帶材交貨技術(shù)條件 | ||||||||
Equivalent grades: | ||||||||
Chemical comb % of steel 2326 | ||||||||
Ti=[4*(C+N)+0.15]至0.80 | ||||||||
可以通過(guò)使用鈦或鈮或鋯來(lái)進(jìn)行穩(wěn)定。根據(jù)這些元素的原子質(zhì)量以及碳和氮的含量,當(dāng)量應(yīng)為:Nb(質(zhì)量%)=Zr(質(zhì)量% | ||||||||
未經(jīng)買(mǎi)方同意,不得故意將本表中未列出的元素添加到鋼材中,除非對(duì)鑄件進(jìn)行精加工。 | ||||||||
C | Si | Mn | P | S | Cr | Mo | N | Ti |
max 0.025 | max 1 | max 1 | max 0.04 | max 0.015 | 17 - 20 | 1.8 - 2.5 | max 0.03 | 0.15 - 0.8 |
Mechanical properties of steel 2326 | ||||||||
Rm - Tensile strength (MPa) (+A) | 400-640 | |||||||
Rp0.2 0.2% proof strength (MPa) (+A) | 280-320 | |||||||
A - Min. elongation at fracture (%) (+A) | 20 | |||||||
Properties of steel 2326 | ||||||||
耐晶間腐蝕:在交貨條件下-是;處于焊接狀態(tài)-是 |